Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of GADEL 2300 - PAEK - Gharda Plastics Limited

Material Data Center offers the following functions for GADEL 2300:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Gadel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
성형 수축률, 평행 0.01 mm/mm ASTM D 955
성형 수축률, 수직 0.011 mm/mm ASTM D 955
기계적 특성단위시험규격
ASTM 데이터
인장탄성률 4100 MPa ASTM D 638
인장 강도 100 MPa ASTM D 638
파단시 신율 6 % ASTM D 638
굴곡 계수 6000 MPa ASTM D 790
굴곡 강도 185 MPa ASTM D 790
쇼어 D 경도 87 - ASTM D 2240
아이조드 충격은 노치, 1/8 in 60 J/m ASTM D 256
Izod충격강도, 1/8 in N J/m ASTM D 256
열적 특성단위시험규격
ASTM 데이터
DTUL @ 264 psi 160 °C ASTM D 648
녹는점 372 °C ASTM D 3418
유리 전이 온도 154 °C ASTM E 1356
기타 특성단위시험규격
밀도 1300 kg/m³ ASTM D 792
특징
생산 공정
기타 압출
특별 특성
열안정성
내화학성에
General Chemical Resistance, Oil Resistance, Radiation Resistance
응용
항공 우주, 자동차의, 화학 공정, 전기 및 전자
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.