Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of HOPELEN SFI-151 - PP - Lotte Chemical Corporation

Material Data Center offers the following functions for HOPELEN SFI-151:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Hopelen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 8 g/10min ISO 1133
ASTM 데이터
용융 흐름성, MFI 8 g/10min ASTM D 1238
기계적 특성단위시험규격
ISO 데이터
항복강도 32 MPa ISO 527
파단시 신율 500 % ISO 527
굴곡 계수, 23°C 1520 MPa ISO 178
로크웰 경도 R 100 - ISO 2039-2
ASTM 데이터
항복강도 35 MPa ASTM D 638
파단시 신율 500 % ASTM D 638
굴곡 계수 1472 MPa ASTM D 790
로크웰 경도 R 102 - ASTM D 785
아이조드 충격은 노치, 1/8 in 39.2 J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 162 °C ISO 11357-1/-3
ASTM 데이터
DTUL @ 66 psi 113 °C ASTM D 648
녹는점 162 °C ASTM D 3418
광학 특성단위시험규격
ASTM 데이터
탁도 2 % ASTM D 1003
기타 특성단위시험규격
밀도 900 kg/m³ ISO 1183
밀도 900 kg/m³ ASTM D 792
특징
특별 특성
투명도
특성
Homopolymer
Certifications
Food contact
응용
포장
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.