Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kocetal® LW301 - POM... - Kolon Industries

Material Data Center offers the following functions for Kocetal® LW301:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kocetal datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 9.5 g/10min ISO 1133
온도 190 °C -
负荷 2.16 kg -
성형 수축률, 평행 2.0 % ISO 294-4, 2577
ASTM 데이터
용융 흐름성, MFI 10 g/10min ASTM D 1238
성형 수축률, 평행 0.02 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
인장 강도 56 MPa ISO 527
파단시 신율 40 % ISO 527
굴곡 계수, 23°C 2500 MPa ISO 178
챠피 노치드 충격 강도, +23°C 7 kJ/m² ISO 179/1eA
로크웰 경도 M 78 - ISO 2039-2
ASTM 데이터
인장 강도 55 MPa ASTM D 638
파단시 신율 60 % ASTM D 638
굴곡 계수 2200 MPa ASTM D 790
굴곡 강도 80 MPa ASTM D 790
로크웰 경도 M 78 - ASTM D 785
아이조드 충격은 노치, 1/8 in 80 J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 166 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 87 °C ISO 75-1/-2
ASTM 데이터
UL94 난연성 HB - UL 94
테스트 두께 0.8 mm -
열팽창 계수, 평행 130 E-6/K ASTM D 696
DTUL @ 66 psi 158 °C ASTM D 648
DTUL @ 264 psi 110 °C ASTM D 648
녹는점 166 °C ASTM D 3418
전기적 특성단위시험규격
ISO 데이터
부피 저항 1E12 Ohm*m IEC 62631-3-1
표면 저항 >1E15 Ohm IEC 62631-3-2
전기 압력 19 kV/mm IEC 60243-1
ASTM 데이터
전기 압력, 단기간의 19 kV/mm ASTM D 149
소산 인자, 1 MHz 0.006 - ASTM D 150
표면 저항 >1E15 Ohm ASTM D 257
부피 저항 1E14 Ohm*cm ASTM D 257
기타 특성단위시험규격
밀도 1400 kg/m³ ISO 1183
밀도 1400 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 - 90 °C -
Pre-drying - Time 3 h -
용융수지온도 ≤220 °C -
성형온도 60 - 80 °C -
Zone 1 180 °C -
Zone 2 190 °C -
Zone 3 190 °C -
Nozzle temperature 200 °C -
특징
생산 공정
사출 성형
부가물
윤활제
특성
Tribologic Grade
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.