Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KOPLA® KDG1015F - PA66-GF15 - KOPLA CO., LTD

Material Data Center offers the following functions for KOPLA® KDG1015F:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kopla datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
성형 수축률, 평행 0.0055 mm/mm ASTM D 955
성형 수축률, 수직 0.0085 mm/mm ASTM D 955
기계적 특성건조/응축단위시험규격
ISO 데이터
챠피 충격 강도, +23°C 45 / 52 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 8 / 9 kJ/m² ISO 179/1eA
ASTM 데이터
인장탄성률 5900 / 4600 MPa ASTM D 638
인장 강도 115 / 85 MPa ASTM D 638
굴곡 계수 5500 / 4100 MPa ASTM D 790
굴곡 강도 160 / 100 MPa ASTM D 790
로크웰 경도 R 120 / R 115 - ASTM D 785
열적 특성단위시험규격
ASTM 데이터
UL94 난연성 V-0 - UL 94
열팽창 계수, 평행 35 E-6/K ASTM D 696
DTUL @ 66 psi 238 °C ASTM D 648
DTUL @ 264 psi 220 °C ASTM D 648
녹는점 260 °C ASTM D 3418
전기적 특성건조/응축단위시험규격
ASTM 데이터
전기 압력, 단기간의 40 / - kV/mm ASTM D 149
소산 인자, 1 MHz 0.02 / - - ASTM D 150
상대 유전율, 1 MHz 3 / - - ASTM D 150
부피 저항 1E15 / - Ohm*cm ASTM D 257
기타 특성단위시험규격
물에서의 흡수성, 24hr 0.8 % ASTM D 570
밀도 1450 kg/m³ ASTM D 792
특징
특별 특성
난연성, 열안정성
응용
자동차의, 전기 및 전자
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com