Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LIM® 6040 - VMQ - Momentive Performance Materials Inc.

Material Data Center offers the following functions for LIM® 6040:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other LIM datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Appearance/Color:
liquid, transparent

Characteristics:
fast cure, high tear strength

Conformity:
The product meets the requirements for passing the test standards USP Class VI, FDA 21 CFR 177.2600 and ISO 10993.
Based on listing of ingredients in the BfR recommendation XV "Silicones", the product is compositionally compliant.

These values were determined with the following conditions:
Postbaked 1 hr @ 204ºC / 400ºF.

Other values were achieved with the following conditions:
As Molded 30 sec @ 177ºC / 350ºF:


Property Value Unit Standard
Shore A hardness, 3s 40 - ISO 868
Tensile Strength 8.3 MPa
ISO 37
Strain at break 650 %
ISO 37
Tear Strength 40,4 kN/m
ASTM D 624
기계적 특성단위시험규격
ISO 데이터
인장 강도 9 MPa ISO 37
파단시 신율 600 % ISO 37
쇼어 A 경도 42 - ISO 7619-1
ASTM 데이터
전단강도 39 kN/m ASTM D 624
열적 특성단위시험규격
ISO 데이터
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
Yellow Card 유효한 - -
기타 특성단위시험규격
밀도 1120 kg/m³ ISO 1183
특징
생산 공정
사출 성형
특별 특성
투명도
Certifications
Food contact, Food approval BfR, Food approval FDA 21 CFR, US Pharmacopeia Class VI Approved
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.