Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOY HI5007U - (PC+ABS) - LG Chem

Material Data Center offers the following functions for LUPOY HI5007U:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lupoy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 14 g/10min ISO 1133
온도 260 °C -
负荷 5 kg -
성형 수축률, 평행 0.7 % ISO 294-4, 2577
성형 수축률, 수직 0.7 % ISO 294-4, 2577
ASTM 데이터
용융 흐름성, MFI 3.7 g/10min ASTM D 1238
온도 250 °C -
하중 2.16 kg -
성형 수축률, 평행 0.007 mm/mm ASTM D 955
성형 수축률, 수직 0.007 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
인장탄성률 1800 MPa ISO 527
항복강도 50 MPa ISO 527
항복변형률 4.3 % ISO 527
파단시 강도 54 MPa ISO 527
파단시 신율 120 % ISO 527
굴곡 계수, 23°C 2180 MPa ISO 178
굴곡 강도 75 MPa ISO 178
챠피 노치드 충격 강도, +23°C 59[1] kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 33[1] kJ/m² ISO 179/1eA
아이조드 충격은 노치, +23°C 55[1] kJ/m² ISO 180/1A
아이조드 충격은 노치 18[1] kJ/m² ISO 180/1A
온도 -40 °C -
로크웰 경도 R 115 - ISO 2039-2
ASTM 데이터
인장탄성률 2178 MPa ASTM D 638
항복강도 54 MPa ASTM D 638
파단시 강도 51 MPa ASTM D 638
항복변형률 4.5 % ASTM D 638
파단시 신율 126 % ASTM D 638
굴곡 계수 2083 MPa ASTM D 790
굴곡 강도 87.3 MPa ASTM D 790
로크웰 경도 R 115 - ASTM D 785
아이조드 충격은 노치, 1/8 in 627 J/m ASTM D 256
아이조드 충격은 노치, 1/4 in 471 J/m ASTM D 256
아이조드 충격은 노치, Low-Temperature 255 J/m ASTM D 256
온도 -30 °C -
1: 4 mm
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 94[2] °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 117[2] °C ISO 75-1/-2
비카트 연화 온도, B 113 °C ISO 306
선형 열팽창 계수, 평행 78 E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 81 E-6/K ISO 11359-1/-2
ASTM 데이터
열팽창 계수, 평행 78 E-6/K ASTM D 696
열팽창 계수, 수직 81 E-6/K ASTM D 696
DTUL @ 66 psi 124 °C ASTM D 648
DTUL @ 264 psi 105 °C ASTM D 648
비카트 연화 온도 117 °C ASTM D 1525
2: 4 mm
전기적 특성단위시험규격
ISO 데이터
부피 저항 1E15 Ohm*m IEC 62631-3-1
표면 저항 1E15 Ohm IEC 62631-3-2
ASTM 데이터
전기 압력, 단기간의 25 kV/mm ASTM D 149
표면 저항 1E15 Ohm ASTM D 257
부피 저항 1E17 Ohm*cm ASTM D 257
기타 특성단위시험규격
조건에서의 흡습성 0.2 % ISO 62와 유사
밀도 1130 kg/m³ ISO 1183
밀도 1130 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 - 100 °C -
Pre-drying - Time 4 - 6 h -
Processing humidity ≤0.02 % -
용융수지온도 240 - 260 °C -
성형온도 60 - 80 °C -
Zone 1 240 - 260 °C -
Zone 2 250 - 270 °C -
Zone 3 250 - 270 °C -
Nozzle temperature 250 - 280 °C -
특징
생산 공정
사출 성형
응용
자동차의, 전기 및 전자 , 범용
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.