Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® ECO 388S BC60 - SAN - INEOS Styrolution

Material Data Center offers the following functions for Luran® ECO 388S BC60:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Luran® ECO 388S BC60 is a specialty grade of SAN with enhanced chemical resistance and the highest mechanical strength. It is suitable for injection molding and extrusion applications. Luran® ECO 388S BC60 is an ISCC compliant product leading to a substitution of fossil source styrene with ISCC certified bio-attributed styrene.
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 77 % (ISO 14044)
Attributed Content of ISCC-certified Bio-Circular Sources (min.): 60 %
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 7 cm³/10min ISO 1133
온도 220 °C -
하중 10 kg -
성형 수축률, 평행 0.5 % ISO 294-4, 2577
용융 열전도율 0.17 W/(m K) -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 3800 MPa ISO 527
파단시 강도 79 MPa ISO 527
파단시 신율 4 % ISO 527
굴곡 계수, 23°C 3670 MPa ISO 178
굴곡 강도 140 MPa ISO 178
챠피 충격 강도 , +23°C 21 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 19 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 2.5 kJ/m² ISO 179/1eA
아이조드 충격은 노치, +23°C 2.5 kJ/m² ISO 180/1A
Ball indentation hardness 175 MPa ISO 2039-1
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 101 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 102 °C ISO 75-1/-2
비카트 연화 온도, B 107 °C ISO 306
선형 열팽창 계수, 평행 70 E-6/K ISO 11359-1/-2
Other Standards[S]
열전도율, 솔리드 0.17 W/(m K) DIN 52612-1
S: These properties are reported by the producer according standards that are different to our defaults.
광학 특성단위시험규격
ASTM 데이터
탁도 1 % ASTM D 1003
광선 투겠淅 89 % ASTM D 1003
Other Standards[S]
굴절 지수 1.56 - ISO 489
S: These properties are reported by the producer according standards that are different to our defaults.
기타 특성단위시험규격
조건에서의 흡습성 0.3 % ISO 62와 유사
밀도 1080 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
용융수지온도 220 - 260 °C -
성형온도 40 - 80 °C -
Injection speed 200 mm/s -
Processing Recommendation Extrusion단위시험규격
Type of extrusion profile - -
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
용융수지온도 240 °C -
Type of extrusion sheet - -
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
용융수지온도 220 - 240 °C -
도표
점도-변형률 , Luran® ECO 388S BC60, SAN, INEOS Styrolution
전단-변형률 , Luran® ECO 388S BC60, SAN, INEOS Styrolution
응력-신율 , Luran® ECO 388S BC60, SAN, INEOS Styrolution
시컨트탄성율-신율 , Luran® ECO 388S BC60, SAN, INEOS Styrolution
응력-신율(등시) 23°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
크립탄성율-시간 23°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
곡선 크리프 23°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
응력-신율(등시) 40°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
크립탄성율-시간 40°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
곡선 크리프 40°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
응력-신율(등시) 60°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
크립탄성율 -시간 60°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
곡선 크리프 60°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
응력-신율(등시) 80°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
크립탄성율-시간 80°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
곡선 크리프 80°C, Luran® ECO 388S BC60, SAN, INEOS Styrolution
비용적-온도(pvT) , Luran® ECO 388S BC60, SAN, INEOS Styrolution
인장탄성율-온도 , Luran® ECO 388S BC60, SAN, INEOS Styrolution
특징
생산 공정
사출 성형, 외형 압출, 시트 압출, 기타 압출, 열성형
인도 유형
펠렛 (입자,알갱이)
특별 특성
열안정성, 투명도
내화학성에
General Chemical Resistance
Certifications
Contains renewable resources, Food contact, ISCC Plus
응용
전기 및 전자
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
기타 정보
사E성
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 220 - 260°C

Mold temperature, range: 40 - 80°C

기타 압출
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Prepreg, Melt temperature: 220 - 240°C

Pipes, Melt temperature: 220 - 240°C

프로파일 압
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Profiles, Melt temperature: 240°C

시트 압
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Plates, Melt temperature: 220 - 240°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.