Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of MABLEX® 274SL05 - (PC+ABS+PTFE) - Ravago Group

Material Data Center offers the following functions for MABLEX® 274SL05:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Mablex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 18 g/10min ISO 1133
온도 260 °C -
负荷 5 kg -
ASTM 데이터
성형 수축률, 평행 0.0055 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
항복강도 45 MPa ISO 527
파단시 강도 35 MPa ISO 527
파단시 신율 60 % ISO 527
굴곡 계수, 23°C 2450 MPa ISO 178
아이조드 충격은 노치, +23°C 50 kJ/m² ISO 180/1A
아이조드 충격은 노치 20 kJ/m² ISO 180/1A
온도 -30 °C -
열적 특성단위시험규격
ISO 데이터
비카트 연화 온도, B 121 °C ISO 306
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.6 mm -
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 3.2 mm -
연소속도, FMVSS, 두께 1mm 20 mm/min ISO 3795 (FMVSS 302)
기타 특성단위시험규격
밀도 1150 kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 100 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.05 % -
용융수지온도 250 - 270 °C -
성형온도 50 - 80 °C -
Zone 1 225 - 240 °C -
Zone 2 240 - 260 °C -
Zone 3 260 - 270 °C -
Nozzle temperature 250 - 260 °C -
Screw speed 40 - 70 rpm -
Back pressure 0.3 - 1.5 MPa -
유지압력 3 - 7 MPa -
특징
생산 공정
사출 성형
부가물
윤활제
지역별 검색
짱쨌쨈
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.