Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® ET3113 RE - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® ET3113 RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
  • MVR (300 °C/1.2 kg) 6.0 cm³/10 min
  • Extrusion
  • high viscosity
  • UV stabilized
  • solid sheet
  • corrugated sheet
Partially bio-circular grade / Attributed via mass balance (according to ISCC PLUS Standard).
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 6 cm³/10min ISO 1133
온도 300 °C -
하중 1.2 kg -
용융 흐름성, MFI 6.5 g/10min ISO 1133
온도 300 °C -
负荷 1.2 kg -
성형 수축률, 평행 0.7 % ISO 294-4, 2577
성형 수축률, 수직 0.8 % ISO 294-4, 2577
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2350 MPa ISO 527
항복강도 65 MPa ISO 527
항복변형률 6.3 % ISO 527
파단시 평균신율 >50 % ISO 527
굴곡 계수, 23°C 2350 MPa ISO 178
굴곡 강도 96 MPa ISO 178
탄성변형률, 1h 2200 MPa ISO 899-1
탄성변형률, 1000h 1900 MPa ISO 899-1
챠피 충격 강도 , +23°C N kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C, 3mm 80 kJ/m² ISO 179/1eA
Type of failure P - -
챠피 노치드 충격 강도, -30°C, 3mm 18 kJ/m² ISO 179/1eA
Type of failure C(P) - -
아이조드 충격은 노치, +23°C 70 kJ/m² ISO 180/1A
아이조드 충격은 노치 20 kJ/m² ISO 180/1A
온도 -30 °C -
최대 관통힘, +23°C 5600 N ISO 6603-2
최대 관통힘, -30°C 6500 N ISO 6603-2
관통 에너지, +23°C 60 J ISO 6603-2
관통 에너지, -30°C 70 J ISO 6603-2
Ball indentation hardness 113 MPa ISO 2039-1
열적 특성단위시험규격
ISO 데이터
유리 전이 온도, 10 °C/min 148 °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 128 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 141 °C ISO 75-1/-2
비카트 연화 온도, B 148 °C ISO 306
선형 열팽창 계수, 평행 65 E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 65 E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.5 mm -
Yellow Card 유효한 - -
두께 H인 제품의 난연성 V-2 class IEC 60695-11-10
테스트 두께 0.8 mm -
Yellow Card 유효한 - -
산소지수로서의 난연성 28 % ISO 4589-1/-2
Glow Wire Flammability Index (GWFI) 875 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Flammability Index (GWFI) 875 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 900 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
전기적 특성단위시험규격
ISO 데이터
상대 유전율, 100Hz 3.1 - IEC 62631-2-1
상대 유전뮬, 1MHz 3 - IEC 62631-2-1
소산 인자, 100Hz 8 E-4 IEC 62631-2-1
소산 인자, 1MHz 100 E-4 IEC 62631-2-1
부피 저항 >1E13 Ohm*m IEC 62631-3-1
표면 저항 >1E15 Ohm IEC 62631-3-2
전기 압력 34 kV/mm IEC 60243-1
CTI 250 - IEC 60112
광학 특성단위시험규격
ISO Data
탁도 0.8 - ISO 14782
광선 투겠淅 89 % ISO 13468-1, -2
기타 특성단위시험규격
물에서의 흡수성 0.3 % ISO 62와 유사
조건에서의 흡습성 0.12 % ISO 62와 유사
밀도 1200 kg/m³ ISO 1183
Bulk density 660 kg/m³ -
기계적 성질 (필름) 단위시험규격
ISO 데이터
수증기 투과속도, 23°C/85%RH 15 g/(m²*d) ISO 15106-1/-2
시편두께 0.1 mm -
테스트 견본 생산단위시험규격
ISO 데이터
사출성형: 용융수지온도 300 °C ISO 294
사출성형: 금형온도 80 °C ISO 294
사출성형: 사출속도 200 mm/s ISO 294
특징
생산 공정
사출 성형, 시트 압출, 기타 압출
인도 유형
펠렛 (입자,알갱이)
특별 특성
U.V. 안정성 또는 기후 안정성, 투명도
Certifications
Contains renewable resources, ISCC Plus
지역별 검색
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.