Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Novapol® TR-0338-UI(UIG) - (PE-LLD) - Nova Chemicals Corp.

Material Data Center offers the following functions for Novapol® TR-0338-UI(UIG):
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Novapol datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 3.5 g/10min ASTM D 1238
온도 190 °C -
하중 2.16 kg -
기계적 특성단위시험규격
ASTM 데이터
항복강도 19.4 MPa ASTM D 638
항복변형률 11 % ASTM D 638
열적 특성단위시험규격
ASTM 데이터
UL94 난연성 HB - UL 94
DTUL @ 66 psi 60 °C ASTM D 648
DTUL @ 264 psi 43 °C ASTM D 648
녹는점 125 °C ASTM D 3418
기타 특성단위시험규격
밀도 938 kg/m³ ASTM D 792
특징
생산 공정
회전 성형
특별 특성
고충격 또는 고충격 보강, U.V. 안정성 또는 기후 안정성
특성
Copolymer, Hexene Copolymer
내화학성에
General Chemical Resistance, Environmental Stress Crack Resistance, Oxidation Resistance
Certifications
Food contact, Food approval FDA 21 CFR, Drinking water contact, Drinking water contact NSF 61
응용
범용
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.