Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Novodur® Ultra 4255 - (ABS+PC) - INEOS Styrolution

Material Data Center offers the following functions for Novodur® Ultra 4255:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other Novodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Novodur® Ultra 4255 acrylonitrile butadiene styrene (ABS) polymer features high surface quality and good impact strength. Novodur® Ultra 4255 is PC modified injection molding grade combining very high impact strength at room as well as at low temperature, 100 % ductility at -30 °C, high heat resistance and a best in class flowability. Furthermore, it is of low emission, i.e. suitable to produce parts which fulfill interior emission requirements of the automotive OEMs.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 17 cm³/10min ISO 1133
온도 260 °C -
하중 5 kg -
용융 밀도 966 kg/m³ -
용융 열전도율 0.211 W/(m K) -
용융 비열용량 2250 J/(kg K) -
이형온도 101 °C -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2100 MPa ISO 527
항복강도 47 MPa ISO 527
항복변형률 4.1 % ISO 527
파단시 평균신율 >50 % ISO 527
챠피 충격 강도 , +23°C N kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C N kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 55 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 55 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 103 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 116 °C ISO 75-1/-2
비카트 연화 온도, B 110 °C ISO 306
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.5 mm -
Yellow Card 유효한 - -
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 3.0 mm -
Yellow Card 유효한 - -
전기적 특성단위시험규격
ISO 데이터
전기 압력 35 kV/mm IEC 60243-1
CTI 275 - IEC 60112
기타 특성단위시험규격
밀도 1100 kg/m³ ISO 1183
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
특성
Low Emission
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
기타 정보
사E성
PREPROCESSING

Pre-drying, Temperature: 80 - 90°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 250 - 270°C

Mold temperature, range: 60 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.