Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of P84®UHT 05P DF - PI-Z - Evonik Operations GmbH

Material Data Center offers the following functions for P84®UHT 05P DF:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other P84 datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서

High temperature resistance, unfilled Polyimide

Polyimid P84®UHT - at a glance

 

  • Excellent thermal-oxidative stability (use up to 300 ° C)
  • High mechanical strength and dimensional stability even at very high temperatures
  • Good creep resistance under load even at high temperatures
  • Easy machinability with standard tools for metals
  • Excellent tribological properties, high wear resistance
  • Processing by direct forming

 

Application examples

bushings, seals, bearings components, guides, gear wheels, and valve parts

in the automotive and aerospace industries and in industrial equipment.

For further information please visit WWW.P84.COM.

기계적 특성단위시험규격
ISO 데이터
인장탄성률 5100 MPa ISO 527
파단시 강도 114 MPa ISO 527
파단시 신율 4.2 % ISO 527
챠피 충격 강도 , +23°C 35 kJ/m² ISO 179/1eU
Type of failure C - -
챠피 노치드 충격 강도, +23°C 3 kJ/m² ISO 179/1eA
Type of failure C - -
쇼어 D 경도 87 - ISO 7619-1
열적 특성단위시험규격
ISO 데이터
유리 전이 온도, 10 °C/min 290 °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 267 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 288 °C ISO 75-1/-2
기타 특성단위시험규격
밀도 1360 kg/m³ ISO 1183
특징
생산 공정
트랜스퍼 성형
인도 유형
가루
부가물
이형제
특별 특성
열안정성
특성
Creep Resistance, Thermal Stability, Tribologic Grade
내화학성에
Oxidation Resistance
응용
항공 우주, 자동차의
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.