Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 5513 SP 01 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 5513 SP 01:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Polyether block amide Pebax® 5513 SP 01 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
Added to PA6, Pebax® 5513 SP 01 resin enhances the properties of PA6, especially at low temperatures and low humidity content, at the same time maintaining the transparency of the nylon film and improving its soft touch.
This SP grade has been developed to be heat and UV resistant.


Main applications:
  • PA6 film additive


Packaging:

This grade is delivered dried in sealed packaging (20 kg and 25 kg bags and 454 kg rigid containers) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 - / 180 MPa ISO 527
항복강도 14 / 13 MPa ISO 527
항복변형률 32 / 30 % ISO 527
파단시 평균신율 >50 / >50 % ISO 527
챠피 노치드 충격 강도, -30°C - / 34 kJ/m² ISO 179/1eA
파단시 강도 TPE 60 / * MPa ISO 527
파단시 신율 TPE >300 / * % ISO 527
쇼어 D 경도 54 / * - ISO 7619-1
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 195 / * °C ISO 11357-1/-3
비카트 연화 온도, B 169 / * °C ISO 306
기타 특성건조/응축단위시험규격
물에서의 흡수성 6.7 / * % ISO 62와 유사
조건에서의 흡습성 1.3 / * % ISO 62와 유사
밀도 1090 / 1090 kg/m³ ISO 1183
특징
생산 공정
사출 성형, 기타 압출
인도 유형
펠렛 (입자,알갱이)
특별 특성
도금가능한, 가시광선 안정성, U.V. 안정성 또는 기후 안정성, 열안정성
특성
Blending Resin
지역별 검색
기타 정보
사E성

Processing conditions:

- Typical melt temperature (Min / Recommended / Max): 220°C / 240°C / 260°C.
- Typical mold temperature: 25–60°C.
- Drying time and temperature (only necessary for bags/containers opened for more than two hours): 5-7 hours at 70-90°C.
기타 압출

Processing conditions:

- Typical melt temperature (Min / Recommended / Max): 220°C / 235°C / 250°C.
- Drying time and temperature (only necessary for bags/containers opened for more than two hours): 5-7 hours at 70-90°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.