Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 4533 SP 01 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 4533 SP 01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Polyether block amide Pebax® 4533 SP 01 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This SP grade has been developed to be heat and UV resistant.


Main applications:
  • Flexible injected parts
  • High performance power trasmission belts
  • Silent gears


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 88 / 81 MPa ISO 527
50%변형하에서의 강도 9 / 9 MPa ISO 527
파단시 신율 >50 / >50 % ISO 527
10% 변형시 강도 6 / * MPa ISO 527
100% 변형시 강도 9 / * MPa ISO 527
파단시 강도 TPE 42 / * MPa ISO 527
파단시 신율 TPE >300 / * % ISO 527
23 C, 영구 압축줄음율, 24h 37 / * % ISO 815
전단강도 77 / * kN/m ISO 34-1
내마모성 40 / * mm³ ISO 4649
쇼어 A 경도 90 / * - ISO 7619-1
쇼어 D 경도 41 / * - ISO 7619-1
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 147 / * °C ISO 11357-1/-3
하중하에서의 변형온도, 0.45 MPa 52 / * °C ISO 75-1/-2
선형 열팽창 계수, 평행 200 / * E-6/K ISO 11359-1/-2
전기적 특성건조/응축단위시험규격
ISO 데이터
상대 유전율, 100Hz 9 / - - IEC 62631-2-1
상대 유전뮬, 1MHz 6 / - - IEC 62631-2-1
소산 인자, 100Hz 2090 / - E-4 IEC 62631-2-1
소산 인자, 1MHz 1120 / - E-4 IEC 62631-2-1
부피 저항 1.6E11 / - Ohm*m IEC 62631-3-1
표면 저항 * / 3E12 Ohm IEC 62631-3-2
전기 압력 43 / - kV/mm IEC 60243-1
CTI * / 600 - IEC 60112
기타 특성건조/응축단위시험규격
물에서의 흡수성 1.2 / * % ISO 62와 유사
조건에서의 흡습성 0.4 / * % ISO 62와 유사
밀도 1010 / 1010 kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 60 - 70 °C -
Pre-drying - Time 4 - 6 h -
용융수지온도 200 - 270 °C -
성형온도 10 - 30 °C -
도표
점도-변형률 , Pebax® 4533 SP 01, TPA, ARKEMA
전단-변형률 , Pebax® 4533 SP 01, TPA, ARKEMA
응력-신율 , Pebax® 4533 SP 01 (건조), TPA, ARKEMA
시컨트탄성율-신율 , Pebax® 4533 SP 01 (건조), TPA, ARKEMA
비용적-온도(pvT) , Pebax® 4533 SP 01, TPA, ARKEMA
특징
생산 공정
사출 성형, 필름 압출, 외형 압출, 기타 압출, 트랜스퍼 성형, 주조, 열성형
인도 유형
펠렛 (입자,알갱이)
특별 특성
도금가능한, 가시광선 안정성, U.V. 안정성 또는 기후 안정성, 열안정성, 투명도
지역별 검색
기타 정보
사E성

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 200°C / 240°C / 270°C.
- Typical mold temperature : 10 – 30°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 60-70°C.
기타 압출

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 210°C / 220°C / 230°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 60-70°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com