Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PHARMALENE® FL 20 PH BCA - (PE-LD) - Versalis S.p.A

Material Data Center offers the following functions for PHARMALENE® FL 20 PH BCA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pharmalene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Pharmalene FL 20 PH BA will be bio attributed for 100%.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 2.2 g/10min ISO 1133
온도 190 °C -
负荷 2.16 kg -
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 109 °C ISO 11357-1/-3
비카트 연화 온도, A 90 °C ISO 306
광학 특성단위시험규격
ISO Data
탁도 9 - ISO 14782
ASTM 데이터
광택도 54 - ASTM D 2457
기타 특성단위시험규격
밀도 921 kg/m³ ISO 1183
기계적 성질 (필름) 단위시험규격
ISO 데이터
항복시의 강도, 평행 10 MPa ISO 527-3
항복시의 강도, normal 10 MPa ISO 527-3
파단시 강도, 평행 25 MPa ISO 527-3
파단시 강도, 수직 19 MPa ISO 527-3
최대변형율, 평행 300 % ISO 527-3
최대변형율, 수직 550 % ISO 527-3
다트 낙하 충격, 방법 A 190 g ISO 7765-1
동적마찰계수 0.5 - ISO 8295
압출 유형 blown - -
시편두께 0.04 mm -
Processing Recommendation Extrusion단위시험규격
Type of extrusion blown - -
용융수지온도 160 - 190 °C -
특징
생산 공정
Blown Film Extrusion, 필름 압출, 기타 압출, 중공 성형
인도 유형
펠렛 (입자,알갱이)
Certifications
Contains renewable resources, Food contact, Food approval 10/2011, Food approval FDA 21 CFR, Medical Grade, US Pharmacopeia Class VI Approved, ISCC Plus
응용
의료
지역별 검색
짱쨌쨈
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com