Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Platamid® HX 2627 Pellets - PA* - ARKEMA
Material Data Center offers the following functions for Platamid® HX 2627 Pellets:
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
제품 설명서
Platamid® HX 2627 Pellets
Copolyamide Hot Melt Adhesive
Platamid® HX 2627 Pellets is a
thermoplastic copolyamide hot melt adhesive available in pellet form. This grade has been developed to manufacture hot-melt webs, nets and mono- and multi-filaments.
Platamid® HX 2627 Pellets offers a very good adhesion to all kinds of textile substrates based on native and synthetic fibers. Additionally Platamid® HX 2627 Pellets provide elastomeric properties and high water vapor transmission rate.
AVAILABLE GRADESThis grade is available:
- undried with optical brightener (HX 2627 TA)
PACKAGING
Platamid® HX 2627 TA is delivered in 500 kg sealed big bags (GRVS).
This grade is ready to be processed.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Processing/Physical Characteristics | 건조/응축 | 단위 | 시험규격 |
ISO 데이터 |
용융 부피 - 흐름 속도, MVR |
43 / * |
cm³/10min |
ISO 1133 |
온도 |
130 / * |
°C |
- |
하중 |
2.16 / * |
kg |
- |
열적 특성 | 건조/응축 | 단위 | 시험규격 |
ISO 데이터 |
녹는점, 10°C/min |
125 / * |
°C |
ISO 11357-1/-3 |
특징
인도 유형
펠렛 (입자,알갱이)
특성
Good Adhesion, Copolymer
응용
Monofilament, Multifilament
지역별 검색
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.