Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Plexar PX3060 - (PE-LLD) - LyondellBasell Industries

Material Data Center offers the following functions for Plexar PX3060:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Plexar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 2.2 g/10min ASTM D 1238
온도 190 °C -
하중 2.16 kg -
열적 특성단위시험규격
ASTM 데이터
비카트 연화 온도 100 °C ASTM D 1525
기타 특성단위시험규격
밀도 924 kg/m³ ASTM D 792
기계적 성질 (필름) 단위시험규격
ASTM Data
항복강도, 평행 12.6 MPa ASTM D 882
항복강도, 수직 14.2 MPa ASTM D 882
파단시 강도, 평행 30.1 MPa ASTM D 882
파단시 강도, 수직 23.9 MPa ASTM D 882
항복변형률, 평행 16 % ASTM D 882
항복변형률, 수직 10 % ASTM D 882
파단시 신율 , 평행 760 % ASTM D 882
파단시 신율 , 수직 760 % ASTM D 882
압출 유형 blown - -
시편두께 0.05 mm -
특징
생산 공정
Blown Film Extrusion, 필름 압출, Pipe/Tube Extrusion, 시트 압출, 코팅, 중공 성형, 열성형
인도 유형
펠렛 (입자,알갱이)
특성
Barrier Properties
Certifications
Food contact
응용
포장
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.