Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Promyde® BF933 - PA* - Nurel S.A.

Material Data Center offers the following functions for Promyde® BF933:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Promyde datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 35 cm³/10min ISO 1133
온도 275 °C -
하중 5 kg -
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 200 °C ISO 11357-1/-3
광학 특성단위시험규격
ASTM 데이터
탁도 0.5 % ASTM D 1003
기타 특성단위시험규격
밀도 1110 kg/m³ ISO 1183
Moisture Content 0.1 % -
기계적 성질 (필름) 단위시험규격
ISO 데이터
파단시 강도, 평행 65 MPa ISO 527-3
최대변형율, 평행 400 % ISO 527-3
트라우저 전단강도, 평행 45 N/mm ISO 6383-1
동적마찰계수 0.25 - ISO 8295
수증기 투과속도, 23°C/85%RH 20 g/(m²*d) ISO 15106-1/-2
산소 투과율, 23°C/0%r.h. 25 cm³/(m²*d*bar) ISO 15105-1/-2
산소 투과율, 23°C/85%RH 25 cm³/(m²*d*bar) ISO 15105-1/-2
물질의 비성질단위시험규격
ISO 데이터
점도수 202 cm³/g ISO 307, 1157, 1628
Processing Recommendation Extrusion단위시험규격
Pre-drying - Temperature 75 - 80 °C -
Feed temperature 40 - 50 °C -
Zone 1 210 - 250 °C -
Nozzle temperature 240 - 250 °C -
특징
생산 공정
Blown Film Extrusion, 필름 압출, 열성형
특별 특성
투명도
특성
Barrier Properties
Certifications
Food contact
응용
포장
지역별 검색
짱쨌쨈
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.