Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Purell PE 3020K - (PE-LD) - LyondellBasell Industries

Material Data Center offers the following functions for Purell PE 3020K:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Purell datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 4 g/10min ISO 1133
온도 190 °C -
负荷 2.16 kg -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 300 MPa ISO 527
항복강도 13 MPa ISO 527
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 114 °C ISO 11357-1/-3
비카트 연화 온도, A 97 °C ISO 306
광학 특성단위시험규격
ASTM 데이터
광택도 115 - ASTM D 2457
탁도 7 % ASTM D 1003
기타 특성단위시험규격
밀도 928 kg/m³ ISO 1183
기계적 성질 (필름) 단위시험규격
ISO 데이터
최대변형율, 평행 350 % ISO 527-3
최대변형율, 수직 600 % ISO 527-3
특징
생산 공정
사출 성형, Blown Film Extrusion, 필름 압출
인도 유형
펠렛 (입자,알갱이)
특성
Heat Sealable
내화학성에
General Chemical Resistance
Certifications
Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
응용
의료, 포장
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.