Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RamShine PV701GR216-1 - ABS - Polyram

Material Data Center offers the following functions for RamShine PV701GR216-1:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ramshine datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 34 g/10min ISO 1133
온도 220 °C -
负荷 10 kg -
Other Standards[S]
성형 수축률, 평행 0.6 % Producer Method
S: These properties are reported by the producer according standards that are different to our defaults.
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2200 MPa ISO 527
인장 강도 40 MPa ISO 527
아이조드 충격은 노치, +23°C 20 kJ/m² ISO 180/1A
열적 특성단위시험규격
ISO 데이터
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 3.0 mm -
기타 특성단위시험규격
밀도 1050 kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.1 % -
성형온도 40 - 80 °C -
Feed temperature 60 - 70 °C -
Zone 1 200 - 220 °C -
Zone 2 200 - 220 °C -
Zone 3 210 - 240 °C -
특징
생산 공정
사출 성형
특별 특성
U.V. 안정성 또는 기후 안정성
Certifications
RoHS
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.