Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SLOVAMID®66 GF 25 FRG 5 - PA66-GF25 - Plastcom, spol. s r.o.

Material Data Center offers the following functions for SLOVAMID®66 GF 25 FRG 5:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Slovamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 1 g/10min ISO 1133
온도 275 °C -
负荷 0.325 kg -
성형 수축률, 평행 0.5 % ISO 294-4, 2577
성형 수축률, 수직 1.0 % ISO 294-4, 2577
기계적 특성단위시험규격
ISO 데이터
인장탄성률 8500 MPa ISO 527
인장 강도 165 MPa ISO 527
굴곡 계수, 23°C 7300 MPa ISO 178
챠피 충격 강도, +23°C 65 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 11 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 260 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 240 °C ISO 75-1/-2
비카트 연화 온도, B 250 °C ISO 306
1.5mm 평균두께에서의 난연성 V-0 class IEC 60695-11-10
테스트 두께 1.6 mm -
전기적 특성단위시험규격
ISO 데이터
전기 압력 70 kV/mm IEC 60243-1
CTI 550 - IEC 60112
기타 특성단위시험규격
밀도 1340 kg/m³ ISO 1183
Moisture Content 0.15 % -
특징
생산 공정
사출 성형
인도 유형
검정, 자연 색상
부가물
난연제
특별 특성
난연성
응용
전기 및 전자
지역별 검색
짱쨌쨈
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.