Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS 165N - PS - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS 165N:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Styrolution® PS 165N is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 3.4 cm³/10min ISO 1133
온도 200 °C -
하중 5 kg -
용융 밀도 936 kg/m³ -
용융 열전도율 0.155 W/(m K) -
용융 비열용량 2300 J/(kg K) -
이형온도 82 °C -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 3300 MPa ISO 527
파단시 강도 52 MPa ISO 527
파단시 신율 2 % ISO 527
탄성변형률, 1h 3300 MPa ISO 899-1
탄성변형률, 1000h 2600 MPa ISO 899-1
챠피 노치드 충격 강도, +23°C 3 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
유리 전이 온도, 10 °C/min 90 °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 76 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 84 °C ISO 75-1/-2
비카트 연화 온도, B 89 °C ISO 306
선형 열팽창 계수, 평행 80 E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.5 mm -
Yellow Card 유효한 - -
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 3.2 mm -
Yellow Card 유효한 - -
산소지수로서의 난연성 18 % ISO 4589-1/-2
전기적 특성단위시험규격
ISO 데이터
상대 유전율, 100Hz 2.5 - IEC 62631-2-1
상대 유전뮬, 1MHz 2.5 - IEC 62631-2-1
소산 인자, 100Hz 0.9 E-4 IEC 62631-2-1
소산 인자, 1MHz 0.7 E-4 IEC 62631-2-1
CTI 375 - IEC 60112
기타 특성단위시험규격
밀도 1040 kg/m³ ISO 1183
물질의 비성질단위시험규격
ISO 데이터
점도수 119 cm³/g ISO 307, 1157, 1628
테스트 견본 생산단위시험규격
ISO 데이터
사출성형: 용융수지온도 230 °C ISO 294
사출성형: 금형온도 40 °C ISO 294
사출성형: 사출속도 200 mm/s ISO 294
도표
점도-변형률 , Styrolution® PS 165N, PS, INEOS Styrolution
전단-변형률 , Styrolution® PS 165N, PS, INEOS Styrolution
응력-신율 , Styrolution® PS 165N, PS, INEOS Styrolution
시컨트탄성율-신율 , Styrolution® PS 165N, PS, INEOS Styrolution
응력-신율(등시) 23°C, Styrolution® PS 165N, PS, INEOS Styrolution
크립탄성율-시간 23°C, Styrolution® PS 165N, PS, INEOS Styrolution
곡선 크리프 23°C, Styrolution® PS 165N, PS, INEOS Styrolution
비용적-온도(pvT) , Styrolution® PS 165N, PS, INEOS Styrolution
인장탄성율-온도 , Styrolution® PS 165N, PS, INEOS Styrolution
특징
생산 공정
사출 성형, 필름 압출, 외형 압출, 시트 압출, 기타 압출
인도 유형
펠렛 (입자,알갱이)
특별 특성
투명도
지역별 검색
짱쨌쨈, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
기타 정보
사E성
PROCESSING
injection molding, Melt temperature, range: 180 - 280 °C
injection molding, Melt temperature, recommended: 230 °C
injection molding, Mold temperature, range: 10 - 60 °C
injection molding, Mold temperature, recommended: 40 °C

Polystyrol 165N can be injection molded at temperatures between 180 and 280°C.Recommended mold temperatures are between 10 and 60°C.
필름 압출
PROCESSING
Extrusion, Blown film, Melt temperature: 180 - 210 °C
Extrusion, Flat film, Melt temperature: 200 - 240 °C

Extrusion melt temperature should not exceed 240°C.
기타 압출
PROCESSING
Extrusion, Pipes, Melt temperature: 180 - 210 °C
프로파일 압
PROCESSING
Extrusion, Profiles, Melt temperature: 210 °C
시트 압
PROCESSING
Extrusion, Plates, Melt temperature: 200 - 230 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.