Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of STYRON™ 636 BT - PS - Trinseo

Material Data Center offers the following functions for STYRON™ 636 BT:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Styron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 3.1 g/10min ISO 1133
온도 200 °C -
负荷 5 kg -
기계적 특성단위시험규격
ISO 데이터
항복강도 55 MPa ISO 527
파단시 신율 2 % ISO 527
굴곡 계수, 23°C 3500 MPa ISO 178
굴곡 강도 80 MPa ISO 178
로크웰 경도 R 105 - ISO 2039-2
Ball indentation hardness 150 MPa ISO 2039-1
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 90[ann.] °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 93[ann.] °C ISO 75-1/-2
비카트 연화 온도, A 96.5 °C ISO 306
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.6 mm -
ann.: annealed
전기적 특성단위시험규격
ASTM 데이터
소산 인자, 1 MHz 6.0E-5 - ASTM D 150
상대 유전율, 1 MHz 2.5 - ASTM D 150
기타 특성단위시험규격
밀도 1050 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
특징
생산 공정
사출 성형, 기타 압출, 열성형
특성
Blending Resin, Foamable
Certifications
Food contact, Food approval 10/2011, Food approval FDA 21 CFR
응용
범용, 포장, 냉각
지역별 검색
짱쨌쨈, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com