Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Topthane™ 2190E - TPU - Top Polymer Enterprise

Material Data Center offers the following functions for Topthane™ 2190E:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Topthane datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
For more detailed information, please read our brochure
or contact our representatives in your region.
기계적 특성단위시험규격
ASTM 데이터
100% 변형시 탄성률 10.7 MPa ASTM D 412
300% 변형시 탄성률 6.8 MPa ASTM D 412
쇼어 A 경도 90 - ASTM D 2240
전단강도 96.9 kN/m ASTM D 624
파단시 강도 40.8 MPa ASTM D 412
파단시 신율 600 % ASTM D 412
기타 특성단위시험규격
밀도 1180 kg/m³ ASTM D 792
Processing Recommendation Extrusion단위시험규격
Type of extrusion wire/cable - -
Pre-drying - Temperature 90 - 110 °C -
Pre-drying - Time 3 - 4 h -
Zone 1 180 - 190 °C -
Zone 2 190 - 210 °C -
Zone 3 200 - 220 °C -
특징
생산 공정
Pipe/Tube Extrusion, 기타 압출
인도 유형
펠렛 (입자,알갱이)
내화학성에
General Chemical Resistance, Oil Resistance
응용
전기 및 전자 , 스포츠 장비
지역별 검색
쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.