Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ FX100 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ FX100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서

Eastman Tritan™ FX100 is a copolyester resin for extruded film applications where enhanced heat resistance and toughness are required. It works great in high temperature packaging, transaction and identification cards, and

protective laminates.

Packaging brands and film converters prefer Tritan™ FX100 for its ability to provide a clear, aesthetically pleasing package that stands up to the strenuous requirements for hot filling, while also providing safety that consumers expect. It’s great for brands looking to replace materials of concern or premiumize their packaging by transitioning from opaque to clear.

Transaction and identification card producers, brands, and governments alike value Tritan™ FX100 for its excellent bend strength and chemical resistance, which provides longer useful life and better security. Compared to PVC and other material alternatives. Transaction cards made with Tritan™ have been found to withstand more than 10 times the number of flexural cycles using industry standard fitness for use testing protocols.

Tritan™ FX100 may be used in various food contact applications under the U.S. Food & Drug Administration (FDA) regulations.

열적 특성단위시험규격
ASTM 데이터
열팽창 계수, 평행 90 E-6/K ASTM D 696
유리 전이 온도 110 °C ASTM E 1356
광학 특성단위시험규격
ASTM 데이터
광택도 161 - ASTM D 2457
탁도 0.7 % ASTM D 1003
광선 투겠淅 92 % ASTM D 1003
굴절 지수 1.55 - ASTM D 542
기타 특성단위시험규격
물에서의 흡수성, 24hr 0.5 % ASTM D 570
밀도 1190 kg/m³ ASTM D 792
기계적 성질 (필름) 단위시험규격
ISO 데이터
트라우저 전단강도, 평행 11 N/mm ISO 6383-1
트라우저 전단강도, 수직 11 N/mm ISO 6383-1
시편두께 0.254 mm -
ASTM Data
인장탄성률, 평행 1500 MPa ASTM D 882
인장탄성률, 수직 1400 MPa ASTM D 882
항복강도, 평행 41 MPa ASTM D 882
항복강도, 수직 40 MPa ASTM D 882
파단시 강도, 평행 59 MPa ASTM D 882
파단시 강도, 수직 52 MPa ASTM D 882
항복변형률, 평행 7 % ASTM D 882
항복변형률, 수직 7 % ASTM D 882
파단시 신율 , 평행 179 % ASTM D 882
파단시 신율 , 수직 203 % ASTM D 882
시편두께 0.254 mm -
특징
생산 공정
기타 압출
특별 특성
열안정성, 투명도
특성
Amorphous, High Gloss, Scratch Resistant, Copolymer
내화학성에
General Chemical Resistance
Certifications
Food contact, Food approval FDA 21 CFR
응용
포장
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.