Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ MXF121 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ MXF121:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서

Eastman Tritan™ MXF121 copolyester is an amorphous opaque product. Tritan MXF121 contains a mold release derived from vegetable based sources. Tritan MXF121 has many outstanding features that include excellent toughness, hydrolytic stability, heat resistance, chemical resistance, and melt flowability. Tritan MXF121 has been formulated for medical devices. Tritan MXF121 has passed FDA/ISO 10993 testing for cytotoxicity, skin sensitization, and intracutaneous reactivity.

Processing/Physical Characteristics단위시험규격
ASTM 데이터
성형 수축률, 평행 0.0045 mm/mm ASTM D 955
기계적 특성단위시험규격
ASTM 데이터
인장탄성률 1605 MPa ASTM D 638
항복강도 43 MPa ASTM D 638
파단시 강도 47 MPa ASTM D 638
항복변형률 6 % ASTM D 638
파단시 신율 133 % ASTM D 638
굴곡 계수 1748 MPa ASTM D 790
로크웰 경도 R 109 - ASTM D 785
아이조드 충격은 노치, 1/8 in 183 J/m ASTM D 256
Izod충격강도, 1/8 in N J/m ASTM D 256
열적 특성단위시험규격
ASTM 데이터
UL94 난연성 V-2 - UL 94
테스트 두께 1.5 mm -
DTUL @ 66 psi 94 °C ASTM D 648
DTUL @ 264 psi 83 °C ASTM D 648
기타 특성단위시험규격
밀도 1190 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 88 °C -
Pre-drying - Time 4 - 6 h -
용융수지온도 250 - 275 °C -
성형온도 24 - 66 °C -
특징
생산 공정
사출 성형
부가물
이형제
특별 특성
열안정성
특성
Amorphous, Copolymer
내화학성에
General Chemical Resistance, Hydrolytically Stable
Certifications
Food contact, Food approval FDA 21 CFR, Medical Grade, Biocompatibility ISO 10993
응용
의료
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.