Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 4520 LI - PBT - BASF

Material Data Center offers the following functions for Ultradur® B 4520 LI:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Middle viscosity extrusion grade with an exceptionally high melt strength for the extrusion of profiles, films, hollow rods, pipes and blow molded parts.

Abbreviated designation according to ISO 1043-1: PBT
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 8.5 cm³/10min ISO 1133
온도 250 °C -
하중 2.16 kg -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2500 MPa ISO 527
항복강도 52 MPa ISO 527
항복변형률 3.4 % ISO 527
파단시 평균신율 >50 % ISO 527
챠피 충격 강도 , +23°C 250 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 200 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 5.5 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 5.5 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 55 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 140 °C ISO 75-1/-2
특징
생산 공정
필름 압출, Pipe/Tube Extrusion, 외형 압출, 기타 압출, 중공 성형
특성
Melt Strength
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.