Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PLA - PLA - BASF

Material Data Center offers the following functions for Ultrafuse PLA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 21.2 cm³/10min ISO 1133
온도 220 °C -
하중 5 kg -
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 151 °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min 61 °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 55 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 65 °C ISO 75-1/-2
기타 특성단위시험규격
밀도 1250 kg/m³ ISO 1183
3D Data단위시험규격
Other Standards[S]
인장탄성률, flat 2310 MPa ISO 527
인장탄성률, upright 2130 MPa ISO 527
인장 강도, flat 34.7 MPa ISO 527
인장 강도, upright 21.2 MPa ISO 527
파단시 신율 , flat 4.2 % ISO 527
파단시 신율 , upright 1.2 % ISO 527
굴곡 계수, flat 1860 MPa ISO 178
굴곡 계수, on-edge 1710 MPa ISO 178
굴곡 계수, upright 1720 MPa ISO 178
굴곡 강도, flat 98 MPa ISO 178
굴곡 강도, on-edge 105 MPa ISO 178
굴곡 강도, upright 54.9 MPa ISO 178
챠피 충격 강도 , +23°C, flat 13.2 kJ/m² ISO 179/1eU
챠피 충격 강도, +23°C, on-edge 14.3 kJ/m² ISO 179/1eU
챠피 충격 강도, +23°C, upright 4.3 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C, flat 2.5 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, +23°C, on-edge 1.9 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, +23°C, upright 1.7 kJ/m² ISO 179/1eA
Izod충격강도, +23°C, flat 11 kJ/m² ISO 180/1U
Izod충격강도, +23°C, on-edge 9.6 kJ/m² ISO 180/1U
Izod충격강도, +23°C, upright 4.7 kJ/m² ISO 180/1U
아이조드 충격은 노치, +23°C, flat 3.3 kJ/m² ISO 180/1A
아이조드 충격은 노치, +23°C, on-edge 2.1 kJ/m² ISO 180/1A
아이조드 충격은 노치, +23°C, upright 1.6 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
특징
생산 공정
Additive Manufacturing
인도 유형
Monofilament
특성
Low Warpage
Certifications
Contains renewable resources
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.