Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® Advanced N2U40G7 LS BK - PA9T-GF35 FR - BASF

Material Data Center offers the following functions for Ultramid® Advanced N2U40G7 LS BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
The product is a halogen free flame retardant high temperature polyamide with high flowability, high temperature resistance for surface mount technology (SMT), excellent mechanical properties and high dimension stability, which all make it a perfect fit for E&E applications, especially various thin wall connectors and sockets.
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 25 / * cm³/10min ISO 1133
온도 325 / * °C -
하중 2.16 / * kg -
성형 수축률, 평행 0.2 / * % ISO 294-4, 2577
성형 수축률, 수직 0.8 / * % ISO 294-4, 2577
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 12500 / - MPa ISO 527
파단시 강도 150 / - MPa ISO 527
파단시 신율 2 / - % ISO 527
챠피 충격 강도 , +23°C 60 / - kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 13 / - kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 305 / * °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 275 / * °C ISO 75-1/-2
선형 열팽창 계수, 평행 14 / * E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 62 / * E-6/K ISO 11359-1/-2
전기적 특성건조/응축단위시험규격
ISO 데이터
CTI - / 600 - IEC 60112
기타 특성건조/응축단위시험규격
밀도 1490 / - kg/m³ ISO 1183
물질의 비성질건조/응축단위시험규격
ISO 데이터
점도수 70 / * cm³/g ISO 307, 1157, 1628
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 120 °C -
Pre-drying - Time 6 - 8 h -
Processing humidity ≤0.1 % -
용융수지온도 300 - 330 °C -
성형온도 100 - 140 °C -
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이), 검정
특별 특성
난연성, Halogen-free
응용
전기 및 전자
지역별 검색
기타 정보
사E성
PREPROCESSING
Pre/Post-processing, max. allowed water content: .1 %
Pre/Post-processing, Pre-drying, Temperature: 120 °C
Pre/Post-processing, Pre-drying, Time: 6 - 8 h

PROCESSING
injection molding, Melt temperature, range: 310 - 340 °C
injection molding, Melt temperature, recommended: 330 °C
injection molding, Mold temperature, range: 100 - 160 °C
injection molding, Mold temperature, recommended: 140 °C
injection molding, Dwell time, thermoplastics: 5 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.