Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VECTRA® MT®4310 - LCP-GF30 - Celanese

Material Data Center offers the following functions for VECTRA® MT®4310:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vectra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Vectra® MT4310 VF3001 (natural) is a 30% glass reinforced high flow, LCP grade for injection molding.

Vectra® MT4310 VF3001 (natural) is a special grade developed for medical industry applications and complies with:
  • Food Contact Substance Notification (FCN) No. 742 of the Food and Drug Administration (FDA) and is listed in the Drug Master File (DMF 8464) and the Device Master File (MAF 315)
  • the corresponding EU and national registry regulatory requirements
  • biocompatibility in tests corresponding to USP 23 Class VI/ISO 10993
  • low residual monomers
  • no animal products
Highest temperature capability
Easiest flow
Suitable where very thin walls are required
Used for broad range of SMT applications, with minimal dimensional change
Chemical abbreviation according to ISO 1043-1 : LCP
Inherently flame retardant

Flammability at thickness hV-0-
Processing/Physical Characteristics단위시험규격
ISO 데이터
성형 수축률, 평행 0.1 % ISO 294-4, 2577
성형 수축률, 수직 0.5 % ISO 294-4, 2577
기계적 특성단위시험규격
ISO 데이터
인장탄성률 16000 MPa ISO 527
파단시 강도 160 MPa ISO 527
파단시 신율 1.6 % ISO 527
챠피 노치드 충격 강도, +23°C 40 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 335 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 276 °C ISO 75-1/-2
하중하에서의 변형온도, 8.00 MPa 216 °C ISO 75-1/-2
비카트 연화 온도, B 195 °C ISO 306
선형 열팽창 계수, 평행 7 E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 20 E-6/K ISO 11359-1/-2
두께 H인 제품의 난연성 V-0 class IEC 60695-11-10
산소지수로서의 난연성 45 % ISO 4589-1/-2
전기적 특성단위시험규격
ISO 데이터
상대 유전율, 100Hz 4 - IEC 62631-2-1
상대 유전뮬, 1MHz 3.3 - IEC 62631-2-1
소산 인자, 100Hz 100 E-4 IEC 62631-2-1
소산 인자, 1MHz 250 E-4 IEC 62631-2-1
부피 저항 1E13 Ohm*m IEC 62631-3-1
표면 저항 1E14 Ohm IEC 62631-3-2
전기 압력 32 kV/mm IEC 60243-1
기타 특성단위시험규격
밀도 1610 kg/m³ ISO 1183
도표
응력-신율 , VECTRA® MT®4310, LCP-GF30, Celanese
시컨트탄성율-신율 , VECTRA® MT®4310, LCP-GF30, Celanese
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이), 자연 색상
특별 특성
난연성, 가시광선 안정성, 멸균, 에틸렌 산화물 멸균(EtO), 증기 멸균, Gamma irradiation sterilization
Certifications
Food contact, Food approval BfR, Food approval FDA 21 CFR, Food contact notification (FCN), Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved, Drug Master File, Device Master File
응용
의료
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈
기타 정보
사E성
Vectra resins are well known for their excellent thermal and hydrolytic stability. In order to ensure these properties are optimum, the resin should be dried correctly prior to processing. Vectra LCP MT4310 and MT4350 should be dried at 150°C for a minimum of 6 hours or at 170°C for a minimum of 4 hours in a desiccant dryer.
A three-zone screw evenly divided into feed, compression, and metering zones is preferred. A higher percentage of feed flights may be needed for smaller machines: 1/2 feed, 1/4 compression, 1/4 metering.

Vectra LCPs are shear thinning, their melt viscosity decreases quickly as shear rate increases. For parts that are difficult to fill, the molder can increase the injection velocity to improve melt flow.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.