Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of WONDERLITE PC-6600 - PC - Chi Mei Corporation

Material Data Center offers the following functions for WONDERLITE PC-6600:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Wonderlite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 10 cm³/10min ISO 1133
온도 300 °C -
하중 1.2 kg -
성형 수축률, 평행 0.5 % ISO 294-4, 2577
ASTM 데이터
용융 흐름성, MFI 10 g/10min ASTM D 1238
온도 300 °C -
하중 1.2 kg -
성형 수축률, 평행 0.006 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
항복강도 60 MPa ISO 527
파단시 강도 70 MPa ISO 527
굴곡 계수, 23°C 2300 MPa ISO 178
굴곡 강도 90 MPa ISO 178
챠피 노치드 충격 강도, +23°C 60 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 15 kJ/m² ISO 179/1eA
아이조드 충격은 노치, +23°C 60 kJ/m² ISO 180/1A
아이조드 충격은 노치 15 kJ/m² ISO 180/1A
온도 -30 °C -
ASTM 데이터
항복강도 61.8 MPa ASTM D 638
파단시 신율 100 % ASTM D 638
굴곡 계수 2354 MPa ASTM D 790
굴곡 강도 90.2 MPa ASTM D 790
로크웰 경도 R 122 - ASTM D 785
아이조드 충격은 노치, 1/8 in 689 J/m ASTM D 256
아이조드 충격은 노치, Low-Temperature 149 J/m ASTM D 256
온도 -30 °C -
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 125 °C ISO 75-1/-2
비카트 연화 온도, A 150 °C ISO 306
비카트 연화 온도, B 145 °C ISO 306
선형 열팽창 계수, 평행 67 E-6/K ISO 11359-1/-2
두께 H인 제품의 난연성 V-0 class IEC 60695-11-10
테스트 두께 1.0 mm -
Yellow Card 유효한 - -
두께가 h인 제품의 난연성 등급 5V 5VB class IEC 60695-11-20
테스트 두께 2.0 mm -
Yellow Card 유효한 - -
Glow Wire Flammability Index (GWFI) 930 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM 데이터
DTUL @ 264 psi 125 °C ASTM D 648
비카트 연화 온도 145 °C ASTM D 1525
전기적 특성단위시험규격
ISO 데이터
상대 유전뮬, 1MHz 3 - IEC 62631-2-1
부피 저항 3.6E14 Ohm*m IEC 62631-3-1
표면 저항 9.3E14 Ohm IEC 62631-3-2
ASTM 데이터
전기 압력, 단기간의 1.22 kV/mm ASTM D 149
부피 저항 1E14 Ohm*cm ASTM D 257
기타 특성단위시험규격
밀도 1200 kg/m³ ISO 1183
밀도 1200 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 120 °C -
Pre-drying - Time 4 h -
성형온도 70 - 120 °C -
Feed temperature 230 - 300 °C -
Zone 1 250 - 320 °C -
Nozzle temperature 250 - 310 °C -
특징
생산 공정
사출 성형
특별 특성
난연성, Halogen-free, Opaque
응용
전기 및 전자
지역별 검색
쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.