에서의 아세톤 (23°C)

PEBAX products in general possess good resistance to chemicals.
They may swell in certain solvents and this tendency is
stronger for softer grades.

However, any application which places PEBAX in contact with
chemical must be considered a special case and it is particularly
important to contact our technical departments and, when possible,
to carry out tests under real-life conditions.

more information can be found in the following table
pebax chemical resistance


Disclaimer Chemical Resistance
The chemical resistance data reported here are based on either measured weight/dimensional changes or degree of chemical attack determined from exposure in accordance with one of the relevant established international standards (ISO 175, ISO 11403-3, ISO 4599, ISO 4600, ISO 6252 etc.) or on the supplier´s experiences from successful applications of their products. Due to the application specific nature of the surrounding environment of each part during its service life, the indications provided should be used only for a first assessment; they are not intended to substitute for any testing you may need to conduct. You must make your own determination as to the suitibility of this material for your specific application. Users shall in each case conduct evaluations under actual end-use conditions and/or consult with the resin supplier´s technical representatives.