Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELANEX® 2302 GV1/15 - (PBT+PET)-GF15 - Celanese

Material Data Center offers the following functions for CELANEX® 2302 GV1/15:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Celanex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Chemical abbreviation according to ISO 1043-1: PBT Moulding compound ISO 7792- PBT PET, MGHR, 08-060N, GF15; Polybutylene terephthalate polymer blend with PET, 15 % glass fibre reinforced, injection molded parts with superior gloss. Flammability UL 94 HB minimum thickness 0.85 mm. Recognition by Underwriters Laboratories, USA (UL)

Flammability @1.6mm nom. thickn.HB-
Flammability at thickness h (0.85 mm)HBUL recognition (h)
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 20 cm³/10min ISO 1133
온도 265 °C -
하중 2.16 kg -
성형 수축률, 평행 0.5 % ISO 294-4, 2577
성형 수축률, 수직 0.9 % ISO 294-4, 2577
용융 밀도 1220 kg/m³ -
용융 열전도율 0.15 W/(m K) -
용융 비열용량 1820 J/(kg K) -
이형온도 218 °C -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 6200 MPa ISO 527
파단시 강도 115 MPa ISO 527
파단시 신율 3.5 % ISO 527
챠피 충격 강도 , +23°C 35 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 35 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 6.5 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 6.5 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 255 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 190 °C ISO 75-1/-2
하중하에서의 변형온도, 8.00 MPa 65 °C ISO 75-1/-2
비카트 연화 온도, B 210 °C ISO 306
선형 열팽창 계수, 평행 35 E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.4 mm -
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 0.8 mm -
Yellow Card 유효한 - -
산소지수로서의 난연성 19 % ISO 4589-1/-2
전기적 특성단위시험규격
ISO 데이터
상대 유전율, 100Hz 4.1 - IEC 62631-2-1
상대 유전뮬, 1MHz 4 - IEC 62631-2-1
소산 인자, 100Hz 12 E-4 IEC 62631-2-1
소산 인자, 1MHz 180 E-4 IEC 62631-2-1
부피 저항 >1E13 Ohm*m IEC 62631-3-1
표면 저항 >1E15 Ohm IEC 62631-3-2
전기 압력 28 kV/mm IEC 60243-1
기타 특성단위시험규격
물에서의 흡수성 0.45 % ISO 62와 유사
조건에서의 흡습성 0.15 % ISO 62와 유사
밀도 1430 kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 120 - 140 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
용융수지온도 265 - 275 °C -
성형온도 90 - 100 °C -
도표
점도-변형률 , CELANEX® 2302 GV1/15, (PBT+PET)-GF15, Celanese
전단-변형률 , CELANEX® 2302 GV1/15, (PBT+PET)-GF15, Celanese
동전단탄성율-온도 , CELANEX® 2302 GV1/15, (PBT+PET)-GF15, Celanese
응력-신율 , CELANEX® 2302 GV1/15, (PBT+PET)-GF15, Celanese
시컨트탄성율-신율 , CELANEX® 2302 GV1/15, (PBT+PET)-GF15, Celanese
응력-신율(등시) 23°C, CELANEX® 2302 GV1/15, (PBT+PET)-GF15, Celanese
크립탄성율-시간 23°C, CELANEX® 2302 GV1/15, (PBT+PET)-GF15, Celanese
곡선 크리프 23°C, CELANEX® 2302 GV1/15, (PBT+PET)-GF15, Celanese
응력-신율(등시) 60°C, CELANEX® 2302 GV1/15, (PBT+PET)-GF15, Celanese
크립탄성율-시간 60°C, CELANEX® 2302 GV1/15, (PBT+PET)-GF15, Celanese
곡선 크리프 60°C, CELANEX® 2302 GV1/15, (PBT+PET)-GF15, Celanese
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
부가물
이형제
특별 특성
열안정성
특성
High Gloss
지역별 검색
짱쨌쨈
기타 정보
사E성
To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0,02%. The drying should be done in a dry-air dryer (dew point < -30°C) with a temperature of 120 to 140 °C and a drying time of 2 to 4 hours. In case of longer residence times in the dry-air dryer, the temperature should be reduced to 100°C.
The time between drying and processing should be kept as short as possible. The processing machine feed hopper should be closed during the processing operation.
Melt Temperature 265-275 °C
Mold Temperature *) 90-100 °C
Maximum Barrel Residence Time **) 5-10 min
Injection Speed fast
Peripheral screw speed max.0,3 m/sec
Back Pressure 10-30 bar
Injection Pressure 600-1000 bar
Holding Pressure 400-800 bar
Nozzle Design open design preferred

Injection speed, injection pressure and holding pressure have to be optimized to the individual article geometry. To avoid material degradation during processing low back pressure and minimum screw speed have to be used. Overheating of the material has to be avoided.

Celanese recommends only externally heated hot runner systems.

*) For moulded parts with especially high requirements to the surface quality or dimensional stability, a mold temperature of up to 110 °C can be advantageous.

**) If the cylinder temperatures are higher than the recommended maximum temperatures, the max. residence time in the barrel has to be reduced.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.