Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ChronoThane T™ 93A - TPU - AdvanSource Biomaterials

Material Data Center offers the following functions for ChronoThane T™ 93A:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Chronothane datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
For more detailed information, please read our brochure p. 46 to 54
or contact our representatives in your region.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 14 g/10min ASTM D 1238
온도 205 °C -
하중 3.26 kg -
기계적 특성단위시험규격
ASTM 데이터
인장 강도 37.9 MPa ASTM D 638
파단시 신율 500 % ASTM D 638
쇼어 A 경도 93 - ASTM D 2240
기타 특성단위시험규격
물에서의 흡수성, 평형 1.08 % ASTM D 570
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 71.1 - 93.3 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.05 % -
용융수지온도 182 - 204 °C -
Zone 1 166 - 188 °C -
Zone 2 171 - 193 °C -
Zone 3 177 - 199 °C -
Nozzle temperature 182 - 204 °C -
Processing Recommendation Extrusion단위시험규격
Pre-drying - Temperature 71.1 - 93.3 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.05 % -
용융수지온도 182 - 204 °C -
Zone 1 166 - 188 °C -
Zone 2 171 - 193 °C -
Zone 3 177 - 199 °C -
Nozzle temperature 182 - 204 °C -
특징
생산 공정
사출 성형, 기타 압출
인도 유형
펠렛 (입자,알갱이)
특별 특성
고충격 또는 고충격 보강
Certifications
Contains renewable resources, Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
응용
의료
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.