Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Clyrell RC215M - PP - LyondellBasell Industries

Material Data Center offers the following functions for Clyrell RC215M:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Clyrell datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 10 g/10min ISO 1133
온도 230 °C -
负荷 2.16 kg -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 1050 MPa ISO 527
항복강도 27 MPa ISO 527
항복변형률 10 % ISO 527
파단시 신율 >50 % ISO 527
챠피 노치드 충격 강도, +23°C 3.4 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 1.5 kJ/m² ISO 179/1eA
쇼어 D 경도 66 - ISO 7619-1
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 0.45 MPa 65 °C ISO 75-1/-2
비카트 연화 온도, A 130 °C ISO 306
광학 특성단위시험규격
ASTM 데이터
광택도 90 - ASTM D 2457
탁도 1 % ASTM D 1003
기타 특성단위시험규격
밀도 900 kg/m³ ISO 1183
기계적 성질 (필름) 단위시험규격
ASTM Data
항복강도, 평행 22 MPa ASTM D 882
파단시 강도, 평행 35 MPa ASTM D 882
항복변형률, 평행 10 % ASTM D 882
파단시 신율 , 평행 750 % ASTM D 882
압출 유형 cast - -
시편두께 0.05 mm -
특징
생산 공정
필름 압출
부가물
점착방지제
특성
Heat Sealable, Weldable, Copolymer, Random Copolymer
Certifications
Food contact, Food approval 1935/2004/EC, Food approval 10/2011, Food approval FDA 21 CFR
응용
포장
지역별 검색
짱쨌쨈, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.