Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Deprene 201-80 - (EPDM+PP) - Lingen Plastic Rubber Co., Ltd.

Material Data Center offers the following functions for Deprene 201-80:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Deprene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
기계적 특성단위시험규격
ASTM 데이터
쇼어 A 경도 86 - ASTM D 2240
전단강도 40 kN/m ASTM D 624
압축세트, 22 hr @ 73 °F 25 % ASTM D 395
압축세트, 22 hr @ 158 °F 36 % ASTM D 395
인장 강도 9 MPa ASTM D 412
기타 특성단위시험규격
밀도 930 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
용융수지온도 180 - 200 °C -
성형온도 30 - 80 °C -
Zone 1 150 - 170 °C -
Zone 2 170 - 190 °C -
Zone 3 190 - 220 °C -
Nozzle temperature 190 - 210 °C -
Screw speed 100 - 200 rpm -
Back pressure 0.07 - 0.7 MPa -
Processing Recommendation Extrusion단위시험규격
용융수지온도 160 - 180 °C -
성형온도 170 - 190 °C -
Feed temperature 140 - 150 °C -
Zone 1 150 - 170 °C -
Zone 2 170 - 190 °C -
Zone 3 180 - 200 °C -
특징
생산 공정
사출 성형, 기타 압출
지역별 검색
쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.