Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Dynaflex™ G2706-1000-00 - TPE - Avient Corporation

Material Data Center offers the following functions for Dynaflex™ G2706-1000-00:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Dynaflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 1 g/10min ASTM D 1238
온도 200 °C -
하중 5 kg -
성형 수축률, 평행 0.05 mm/mm ASTM D 955
기계적 특성단위시험규격
ASTM 데이터
100% 변형시 탄성률 0.621 MPa ASTM D 412
300% 변형시 탄성률 0.63 MPa ASTM D 412
쇼어 A 경도 28 - ASTM D 2240
전단강도 14 kN/m ASTM D 624
압축세트, 22 hr @ 73 °F 8 % ASTM D 395
파단시 강도 5.52 MPa ASTM D 412
파단시 신율 660 % ASTM D 412
기타 특성단위시험규격
밀도 890 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
성형온도 15.6 - 37.8 °C -
Zone 1 160 - 199 °C -
Zone 2 171 - 210 °C -
Zone 3 188 - 227 °C -
Nozzle temperature 188 - 227 °C -
Screw speed 25 - 75 rpm -
Injection speed 25.4 - 127 mm/s -
Back pressure 0 - 0.758 MPa -
유지압력 0.931 - 2.07 MPa -
특징
생산 공정
사출 성형, 기타 압출
인도 유형
펠렛 (입자,알갱이)
특별 특성
투명도
특성
Good Adhesion, Soft Feel
Certifications
Food contact, Food approval 10/2011, Food approval FDA 21 CFR, US Pharmacopeia Class VI Approved
응용
자동차의, 의료
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.