Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of EasyWood™ - PLA-W40 - Formfutura BV

Material Data Center offers the following functions for EasyWood™:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other EasyWood datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
Other Standards[S]
용융 흐름성, MFI 4.5 g/10min
S: These properties are reported by the producer according standards that are different to our defaults.
기계적 특성단위시험규격
Other Standards[S]
굴곡 계수 2584 MPa
굴곡 강도 59.6 MPa
S: These properties are reported by the producer according standards that are different to our defaults.
열적 특성단위시험규격
ASTM 데이터
녹는점 145 °C ASTM D 3418
기타 특성단위시험규격
밀도 1200 kg/m³ ASTM D 792
기계적 성질 (필름) 단위시험규격
ASTM Data
인장탄성률, 평행 1930 MPa ASTM D 882
인장 강도, 평행 71 MPa ASTM D 882
파단시 신율 , 평행 171 % ASTM D 882
특징
생산 공정
Additive Manufacturing
인도 유형
Monofilament
특성
Low Warpage
Certifications
Contains renewable resources
지역별 검색
짱쨌쨈
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.