Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ECOZEN® Claro 300 - Copolyester - SK Chemicals

Material Data Center offers the following functions for ECOZEN® Claro 300:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ecozen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
ECOZEN® Claro is a semi-crystalline Copolyester grade, offering a combination of great clarity and chemical resistance.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
성형 수축률, 평행 0.0035 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
항복강도 51 MPa ISO 527
항복변형률 4.4 % ISO 527
파단시 강도 56 MPa ISO 527
파단시 신율 343 % ISO 527
굴곡 계수, 23°C 2110 MPa ISO 178
굴곡 강도 73 MPa ISO 178
아이조드 충격은 노치, +23°C 7 kJ/m² ISO 180/1A
로크웰 경도 R 115 - ISO 2039-2
ASTM 데이터
항복강도 50.5 MPa ASTM D 638
파단시 강도 55.9 MPa ASTM D 638
항복변형률 5 % ASTM D 638
파단시 신율 343 % ASTM D 638
굴곡 계수 2238 MPa ASTM D 790
굴곡 강도 74.9 MPa ASTM D 790
로크웰 경도 R 115 - ASTM D 785
아이조드 충격은 노치, 1/8 in 90 J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 0.45 MPa 73 °C ISO 75-1/-2
ASTM 데이터
DTUL @ 66 psi 73 °C ASTM D 648
광학 특성단위시험규격
ASTM 데이터
탁도 1 % ASTM D 1003
광선 투겠淅 85 % ASTM D 1003
기타 특성단위시험규격
밀도 1320 kg/m³ ISO 1183
밀도 1320 kg/m³ ASTM D 792
특징
생산 공정
사출 성형
특별 특성
투명도
특성
Copolymer
내화학성에
General Chemical Resistance
Certifications
Food contact, RoHS
응용
포장
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.