Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastollan® 1264 DU - (TPU-ARET) - BASF Polyurethanes GmbH

Material Data Center offers the following functions for Elastollan® 1264 DU:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Elastollan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
DESCRIPTION
Elastollan 1264 DU is a polyether based TPU

SPECIAL PROPERTIES
transparent, outstanding hydrolysis resistance, low temperature
flexibility and high resistance to micro-organisms
Processable by injection moulding.

TYPICAL APPLICATIONS
ski boots

OTHER HINTS
predrying: 3h at 90 - 110°C in dehumified air dryer.
Additives have to be dried together with granulate.
max. content of humidity before processing: 0,02%
annealing: 20h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
기계적 특성단위시험규격
ISO 데이터
100% 변형시 강도 25 MPa ISO 527
300% 변형시 강도 35 MPa ISO 527
파단시 강도 TPE 50 MPa ISO 527
파단시 신율 TPE >300 % ISO 527
23 C, 영구 압축줄음율, 24h 48 % ISO 815
70 C, 영구 압축줄음율, 24h 48 % ISO 815
전단강도 170 kN/m ISO 34-1
내마모성 40 mm³ ISO 4649
쇼어 D 경도 64 - ISO 7619-1
기타 특성단위시험규격
밀도 1200 kg/m³ ISO 1183
기타 정보
사E성
Barrel temperature : 210 - 225 °C
Melt temperature : 225 °C
Mold temperature: 40 - 60 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.