Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ELITE™ 5401GT - PE - The Dow Chemical Company

Material Data Center offers the following functions for ELITE™ 5401GT:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Elite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 1 g/10min ISO 1133
온도 190 °C -
负荷 2.16 kg -
열적 특성단위시험규격
ASTM 데이터
녹는점 123 °C ASTM D 3418
비카트 연화 온도 100 °C ASTM D 1525
광학 특성단위시험규격
ISO Data
탁도 13 - ISO 14782
ASTM 데이터
광택도 64 - ASTM D 2457
기타 특성단위시험규격
밀도 917 kg/m³ ASTM D 792
기계적 성질 (필름) 단위시험규격
ISO 데이터
항복시의 강도, 평행 8 MPa ISO 527-3
항복시의 강도, normal 9 MPa ISO 527-3
파단시 강도, 평행 38 MPa ISO 527-3
파단시 강도, 수직 37 MPa ISO 527-3
최대변형율, 평행 570 % ISO 527-3
최대변형율, 수직 610 % ISO 527-3
다트 낙하 충격, 방법 B 850 g ISO 7765-1
압출 유형 blown - -
시편두께 0.051 mm -
특징
생산 공정
Blown Film Extrusion, 필름 압출
부가물
점착방지제
특별 특성
고충격 또는 고충격 보강
특성
Heat Sealable, Copolymer
Certifications
Food contact, Food approval 10/2011, Food contact notification (FCN)
응용
포장
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.