Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ferrex GPP35CN - PP-K36 - LyondellBasell Industries

Material Data Center offers the following functions for Ferrex GPP35CN:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ferrex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 21 g/10min ASTM D 1238
온도 230 °C -
하중 2.16 kg -
기계적 특성단위시험규격
ASTM 데이터
항복강도 24.1 MPa ASTM D 638
파단시 신율 33 % ASTM D 638
굴곡 계수 2413 MPa ASTM D 790
쇼어 D 경도 67 - ASTM D 2240
Gardner충격 5.65 J ASTM D 2794,4226,5420
아이조드 충격은 노치, 1/8 in 26.7 J/m ASTM D 256
Izod충격강도, 1/8 in 534 J/m ASTM D 256
열적 특성단위시험규격
ASTM 데이터
DTUL @ 66 psi 107 °C ASTM D 648
DTUL @ 264 psi 60 °C ASTM D 648
기타 특성단위시험규격
밀도 1200 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 93.3 °C -
Pre-drying - Time 2 - 3 h -
성형온도 46.1 - 60 °C -
Zone 1 199 - 204 °C -
Zone 2 204 - 210 °C -
Zone 3 210 - 216 °C -
Nozzle temperature 216 - 221 °C -
Screw speed 100 - 150 rpm -
Back pressure 0.138 - 0.345 MPa -
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
특별 특성
고충격 또는 고충격 보강
특성
High Gloss
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.