Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Genestar™ N1000A-M41 - PA9T - Kuraray Co., Ltd.

Material Data Center offers the following functions for Genestar™ N1000A-M41:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Genestar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서

Genestar N1000A-M41 (Black, Natural) is standard, unreinforced injection molding grade provided as pellets..


The main features are:

  • Mechanical properties at high temperature
  • Low water absorption and retention of its initial properties

This grade is suitable for:
  • Friction and wear application
  • Gears
  • Parts in harsh chemical and thermal environments



Processing/Physical Characteristics단위시험규격
ISO 데이터
성형 수축률, 평행 1.4 % ISO 294-4, 2577
성형 수축률, 수직 1.5 % ISO 294-4, 2577
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2720 MPa ISO 527
항복강도 85 MPa ISO 527
항복변형률 4 % ISO 527
챠피 충격 강도 , +23°C 5 kJ/m² ISO 179/1eU
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 300 °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min 125 °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 125 °C ISO 75-1/-2
ASTM 데이터
열팽창 계수, 평행 62 E-6/K ASTM D 696
열팽창 계수, 수직 60 E-6/K ASTM D 696
기타 특성단위시험규격
물에서의 흡수성 0.25 % ISO 62와 유사
밀도 1140 kg/m³ ISO 1183
도표
응력-신율 , Genestar™ N1000A-M41, PA9T, Kuraray
시컨트탄성율-신율 , Genestar™ N1000A-M41, PA9T, Kuraray
비용적-온도(pvT) , Genestar™ N1000A-M41, PA9T, Kuraray
특징
생산 공정
사출 성형
인도 유형
검정, 자연 색상
부가물
이형제
특별 특성
열안정성
특성
Barrier Properties, Creep Resistance, Fatigue Resistance, High Crystallinity, Thermal Stability, Weldable
내화학성에
Acid Resistance, Alkali Resistance, General Chemical Resistance, Environmental Stress Crack Resistance, Solvent Resistance, Grease Resistance, Hydrolytically Stable, Oil Resistance
응용
자동차의, 범용
지역별 검색
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.