Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ISPLEN® PM284 AV - PP-MX20 - Repsol YPF S.A.

Material Data Center offers the following functions for ISPLEN® PM284 AV:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Isplen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 20 g/10min ISO 1133
온도 230 °C -
负荷 2.16 kg -
성형 수축률, 평행 0.7 % ISO 294-4, 2577
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2000 MPa ISO 527
항복강도 24 MPa ISO 527
항복변형률 4 % ISO 527
파단시 강도 19.5 MPa ISO 527
파단시 신율 25 % ISO 527
굴곡 계수, 23°C 2350 MPa ISO 178
챠피 충격 강도, +23°C 50 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 3 kJ/m² ISO 179/1eA
Izod충격강도, +23°C 40 kJ/m² ISO 180/1U
아이조드 충격은 노치, +23°C 4 kJ/m² ISO 180/1A
쇼어 D 경도 65 - ISO 7619-1
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 59 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 95 °C ISO 75-1/-2
비카트 연화 온도, A 148 °C ISO 306
비카트 연화 온도, B 76 °C ISO 306
기타 특성단위시험규격
밀도 1040 kg/m³ ISO 1183
특징
특별 특성
고충격 또는 고충격 보강, U.V. 안정성 또는 기후 안정성
특성
Copolymer
응용
자동차의
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.