Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of K-Resin® KR01 - SB - INEOS Styrolution

Material Data Center offers the following functions for K-Resin® KR01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other K-Resin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
K-Resin® KR01 processes very well in injection molding, providing good cycle times and design flexibility. Applications range from containers and packaging to medical applications, toys, displays, overcaps and hangers.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 8 cm³/10min ISO 1133
온도 200 °C -
하중 5 kg -
용융 흐름성, MFI 8 g/10min ISO 1133
온도 200 °C -
负荷 5 kg -
용융 밀도 905 kg/m³ -
용융 열전도율 0.184 W/(m K) -
용융 비열용량 2320 J/(kg K) -
이형온도 60 °C -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 1500 MPa ISO 527
항복강도 33 MPa ISO 527
항복변형률 2.8 % ISO 527
굴곡 계수, 23°C 1800 MPa ISO 178
챠피 충격 강도 , +23°C 30 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 1.5 kJ/m² ISO 179/1eA
쇼어 D 경도 69 - ISO 7619-1
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 65 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 78 °C ISO 75-1/-2
비카트 연화 온도, B 65 °C ISO 306
ASTM 데이터
비카트 연화 온도 90 °C ASTM D 1525
광학 특성단위시험규격
ASTM 데이터
광택도 164 - ASTM D 2457
광선 투겠淅 93 % ASTM D 1003
기타 특성단위시험규격
조건에서의 흡습성 0.07 % ISO 62와 유사
밀도 1010 kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 50 °C -
Pre-drying - Time 3 - 4 h -
용융수지온도 180 - 240 °C -
성형온도 30 - 50 °C -
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
특별 특성
투명도
특성
High Gloss, Low Warpage, Copolymer
Certifications
Medical Grade, Device Master File
응용
의료, 포장, 장난감
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
기타 정보
사E성
As a rule, the K-Resin® granules do not have to be pre-dried. However, in the event of unfavorable storage or transportation conditions involving severe temperature fluctuations, moisture can condense on the surface of the granules and this then has to be removed in a pre-drying step. The granules should be pre-dried in a dry-air dryer for 3 to 4 hours at a temperature of about 50°C.

PROCESSING

Melt temperature, range: 180 - 240°C

Mold temperature, range: 30 - 50°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.