Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KEYFLEX BT S5035 - TPC - LG Chem

Material Data Center offers the following functions for KEYFLEX BT S5035:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Keyflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 15 g/10min ASTM D 1238
온도 240 °C -
하중 2.16 kg -
성형 수축률, 평행 0.016 mm/mm ASTM D 955
기계적 특성단위시험규격
ASTM 데이터
파단시 강도 32.4 MPa ASTM D 638
파단시 신율 550 % ASTM D 638
굴곡 계수 343.4 MPa ASTM D 790
쇼어 D 경도 52 - ASTM D 2240
전단강도 142 kN/m ASTM D 624
아이조드 충격은 노치, 1/4 in N J/m ASTM D 256
아이조드 충격은 노치, Low-Temperature N J/m ASTM D 256
온도 -40 °C -
열적 특성단위시험규격
ASTM 데이터
DTUL @ 66 psi 60 °C ASTM D 648
녹는점 220 °C ASTM D 3418
기타 특성단위시험규격
물에서의 흡수성, 24hr 0.6 % ASTM D 570
밀도 1180 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 - 90 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.01 % -
용융수지온도 220 - 250 °C -
성형온도 40 - 60 °C -
Zone 1 220 - 240 °C -
Zone 2 230 - 250 °C -
Zone 3 230 - 250 °C -
Nozzle temperature 230 - 250 °C -
Processing Recommendation Extrusion단위시험규격
Pre-drying - Temperature 80 - 90 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.01 % -
용융수지온도 220 - 250 °C -
Zone 1 220 - 230 °C -
Zone 2 225 - 235 °C -
Zone 3 225 - 235 °C -
Zone 4 230 - 240 °C -
Nozzle temperature 220 - 250 °C -
특징
생산 공정
사출 성형, 기타 압출
인도 유형
검정
응용
자동차의
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com