Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KOPLA® KPL1050 - PP-GF50 - KOPLA CO., LTD

Material Data Center offers the following functions for KOPLA® KPL1050:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kopla datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
성형 수축률, 평행 0.5 % ISO 294-4, 2577
ASTM 데이터
성형 수축률, 평행 0.0045 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
인장탄성률 10000 MPa ISO 527
인장 강도 145 MPa ISO 527
굴곡 계수 10300 MPa ISO 178
굴곡 강도 215 MPa ISO 178
챠피 충격 강도, +23°C 77 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 38 kJ/m² ISO 179/1eA
로크웰 경도 R 110 - ISO 2039-2
ASTM 데이터
인장탄성률 10500 MPa ASTM D 638
인장 강도 165 MPa ASTM D 638
굴곡 계수 10000 MPa ASTM D 790
굴곡 강도 215 MPa ASTM D 790
로크웰 경도 R 110 - ASTM D 785
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 165 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 165 °C ISO 75-1/-2
두께 H인 제품의 난연성 HB class IEC 60695-11-10
ASTM 데이터
UL94 난연성 HB - UL 94
DTUL @ 264 psi 165 °C ASTM D 648
녹는점 165 °C ASTM D 3418
기타 특성단위시험규격
밀도 1310 kg/m³ ISO 1183
밀도 1310 kg/m³ ASTM D 792
특징
특별 특성
고충격 또는 고충격 보강
특성
Creep Resistance, Long fiber reinforced
응용
자동차의
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.