Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S 797SE Q440 - ASA - INEOS Styrolution

Material Data Center offers the following functions for Luran® S 797SE Q440:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Luran® S 797SE Q440 acrylonitrile styrene acrylate (ASA) polymer features high surface quality and good impact strength including enhanced colour fastness. The product delivers superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S 797SE Q440 is an extrusion grade providing high impact strength and enhanced UV resistance. It is suitable for co-extrusion with ABS or PVC enabling a low gloss surface finish.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 5 cm³/10min ISO 1133
온도 220 °C -
하중 10 kg -
용융 밀도 967 kg/m³ -
용융 열전도율 0.204 W/(m K) -
용융 비열용량 2830 J/(kg K) -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 1900 MPa ISO 527
항복강도 41 MPa ISO 527
항복변형률 3.5 % ISO 527
파단시 평균신율 8.6 % ISO 527
챠피 충격 강도 , +23°C 210 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 20 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 5 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 96 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 101 °C ISO 75-1/-2
비카트 연화 온도, A 102 °C ISO 306
비카트 연화 온도, B 92 °C ISO 306
선형 열팽창 계수, 평행 95 E-6/K ISO 11359-1/-2
전기적 특성단위시험규격
ISO 데이터
상대 유전율, 100Hz 3.8 - IEC 62631-2-1
소산 인자, 100Hz 90 E-4 IEC 62631-2-1
기타 특성단위시험규격
조건에서의 흡습성 0.4 % ISO 62와 유사
밀도 1070 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Processing Recommendation Extrusion단위시험규격
Type of extrusion profile - -
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
용융수지온도 200 - 240 °C -
Type of extrusion sheet - -
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
용융수지온도 210 - 250 °C -
특징
생산 공정
외형 압출, 시트 압출, 기타 압출
인도 유형
펠렛 (입자,알갱이)
특별 특성
고충격 또는 고충격 보강, 가시광선 안정성, U.V. 안정성 또는 기후 안정성, 열안정성
내화학성에
General Chemical Resistance
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
기타 정보
사E성
기타 압출
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Pipes, Melt temperature: 200 - 240°C

프로파일 압
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Profiles, Melt temperature: 200 - 240°C

시트 압
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Plates, Melt temperature: 210 - 250°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com