Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S KR2861/1C - (ASA+PC) - INEOS Styrolution

Material Data Center offers the following functions for Luran® S KR2861/1C:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Luran® SC KR2861/1C is a blend of ASA with PC, shows high heat and high impact resistance and long-term property retention. Its UV resistance is not only sufficient for all kind of interior applications – incl. unpainted surfaces in light colors – but also for exterior parts with medium weatherability requirements. Luran® S KR2861/1C provides very good impact properties at low temperatures as well as high toughness also in combination with a very high concentration of colorants.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 14 cm³/10min ISO 1133
온도 260 °C -
하중 5 kg -
용융 열전도율 0.18 W/(m K) -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2300 MPa ISO 527
항복강도 53 MPa ISO 527
항복변형률 4.9 % ISO 527
파단시 평균신율 >50 % ISO 527
챠피 노치드 충격 강도, +23°C 65 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 20 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 106 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 125 °C ISO 75-1/-2
비카트 연화 온도, B 120 °C ISO 306
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.5 mm -
Yellow Card 유효한 - -
기타 특성단위시험규격
물에서의 흡수성 0.9 % ISO 62와 유사
조건에서의 흡습성 0.25 % ISO 62와 유사
밀도 1150 kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 100 - 110 °C -
Pre-drying - Time 2 - 4 h -
용융수지온도 260 - 300 °C -
성형온도 60 - 90 °C -
도표
점도-변형률 , Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
전단-변형률 , Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
동전단탄성율-온도 , Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
응력-신율 , Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
시컨트탄성율-신율 , Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
응력-신율(등시) 23°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
크립탄성율-시간 23°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
곡선 크리프 23°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
응력-신율(등시) 40°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
크립탄성율-시간 40°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
곡선 크리프 40°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
응력-신율(등시) 60°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
크립탄성율 -시간 60°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
곡선 크리프 60°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
응력-신율(등시) 80°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
크립탄성율-시간 80°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
곡선 크리프 80°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
응력-신율(등시) 100°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
크립탄성율-시간 100°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
곡선 크리프 100°C, Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
비용적-온도(pvT) , Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
인장탄성율-온도 , Luran® S KR2861/1C, (ASA+PC), INEOS Styrolution
특징
생산 공정
사출 성형, 외형 압출, 시트 압출, 중공 성형, 열성형
인도 유형
펠렛 (입자,알갱이)
부가물
이형제
특별 특성
가시광선 안정성, U.V. 안정성 또는 기후 안정성, 열안정성
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
기타 정보
사E성
PREPROCESSING

Pre-drying, Temperature: 100 - 110°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 260 - 300°C

Mold temperature, range: 60 - 90°C

프로파일 압
PREPROCESSING

Pre-drying, Temperature: 100 - 110°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature: 200 - 240°C

시트 압
PREPROCESSING

Pre-drying, Temperature: 100 - 110°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature: 250 - 280°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.