Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NIPLENE F30 AGR HF - PP-GF30 - Soredi S.p.a.

Material Data Center offers the following functions for NIPLENE F30 AGR HF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Niplene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 10 g/10min ASTM D 1238
온도 230 °C -
하중 2.16 kg -
성형 수축률, 평행 0.004 mm/mm ASTM D 955
성형 수축률, 수직 0.006 mm/mm ASTM D 955
기계적 특성단위시험규격
ASTM 데이터
파단시 강도 90 MPa ASTM D 638
굴곡 계수 6000 MPa ASTM D 790
굴곡 강도 140 MPa ASTM D 790
로크웰 경도 R 113 - ASTM D 785
아이조드 충격은 노치, 1/8 in 125 J/m ASTM D 256
아이조드 충격은 노치, Low-Temperature 76.9 J/m ASTM D 256
온도 -20 °C -
열적 특성단위시험규격
ISO 데이터
선형 열팽창 계수, 수직 30 E-6/K ISO 11359-1/-2
ASTM 데이터
UL94 난연성 HB - UL 94
테스트 두께 1.6 mm -
DTUL @ 264 psi 153 °C ASTM D 648
비카트 연화 온도 144 °C ASTM D 1525
전기적 특성단위시험규격
ISO 데이터
상대 유전뮬, 1MHz 2.7 - IEC 62631-2-1
부피 저항 1E13 Ohm*m IEC 62631-3-1
표면 저항 1E14 Ohm IEC 62631-3-2
전기 압력 60 kV/mm IEC 60243-1
기타 특성단위시험규격
조건에서의 흡습성 0.1 % ISO 62와 유사
밀도 1120 kg/m³ ASTM D 792
특징
특성
Chemically Coupled Reinforcement, Homopolymer
지역별 검색
짱쨌쨈
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com